Correct Use Of Defoamers

Apr 01, 2025

Leave a message

The key to the correct use of defoamers is to choose the right type, control the dosage, use the right addition method, and pay attention to system compatibility and operating conditions. ‌

Specific steps and precautions:
Choose the right type of defoamer
‌Choose the defoamer category according to the system properties (pH, temperature, chemical composition, etc.): ‌
‌Silicon type: good defoaming effect and low dosage, but may cause shrinkage and other problems. ‌Polyether type: high temperature and acid and alkali resistance, but the effect is weak. ‌Mineral oil type: low cost but may affect the transparency of the system. ‌Conduct small and pilot tests when necessary to evaluate the defoaming effect and the impact on the system: for example, simulate actual conditions in the laboratory and production line.
Determine the best dosage ‌Refer to the instructions (usually 0.01%-1%) and adjust according to the actual severity of the foam ‌: ‌Too little dosage will not defoam, too much may cause shrinkage or stratification, and a balance point needs to be found through experiments.
‌Industrial fields allow continuous addition until the foam is eliminated, but food additives must strictly follow the standards‌.
Use the correct addition method ‌It is most effective to add before the foam is generated‌: for example, adding culture medium before fermentation or adding raw materials before mixing the paint.
‌Add in batches‌: Suitable for severe foam, such as adding in batches in different sections of papermaking.
‌Add after dilution‌: High-concentration defoamers need to be diluted with uncontaminated tap water (hot water is prohibited), and the active content is controlled at 5%-10%.
‌Addition methods in different forms‌: ‌Liquid‌: drip or spray.
‌Solid‌: Place at the sewage outlet for decomposition.
‌Powder‌: Professionals add diluent regularly.
Precautions ‌Avoid excessive dosage‌: It may cause shrinkage, fish eyes or affect the gloss of the product.
‌Moderate stirring speed‌: Too fast will introduce new foam, too slow will cause uneven dispersion.
‌Temperature effect‌: Some defoamers are less active at high temperatures.
‌Compatibility test‌: Ensure that there are no adverse reactions before applying the new system.
For example, fatty acids are effective under acidic conditions, but may become foaming agents under alkaline conditions.
‌Safety precautions‌: Some defoamers are irritating to the skin or eyes.